I conducted polymerization tests by 3D printing a 10 x 10 x 0.04 mm CAD model from a suspension prepared using sixty-minute-milled LHS powders, acrylate-based polymers, and photoinitiators.
Printer used: Elegoo Mars 4 DLP
The first test conducted showed the adhesion of cured suspension to the build plate.
In subsequent tests, no adhesion was found.
What I have done so far: changed the films on the resin tank, roughened the build plate's surface, changed suspension (increased and reduced regolith mass %), and increased exposure time for burn-in layers.