10 Questions 8 Answers 0 Followers
Questions related from Amit Kumar Singh Chauhan
If peak broadening can happen due to solid solution and strain, then why we measure crystallite size using williamson hall method which uses the same peak broadening concept. How this method is...
07 August 2023 588 2 View
My current research area is Air jet erosion of additive manufactured Ti6Al4V alloy. if possible then please send me some papers on Air jet erosion of additive manufactured Ti6Al4V alloy.
10 September 2018 6,289 1 View
I have been researching recently in metals for aerospace engineering (fatigue application based) related to additive manufacturing. They are being printed with the enormous cost for a very small...
21 June 2017 6,031 2 View
In the material assignment section, I am not able to define the strain life properties of materials (i.e. Strength Coefficient, Strength Exponent, Ductility Coefficient, Ductility Exponent, Cyclic...
29 May 2017 1,470 3 View
I am currently researching on Ti6Al4V (aerospace applications based) by SLS. Can anyone one suggest me the constraints and challenges to be faced in the same? and also the remedies for those...
09 February 2017 7,782 5 View
I want to kno that for d same total flow rate, what happens to turbine generatr o/p of a vapour pwr plant if HP heatr group bypass line is opened? Thus d plant H.R. Increase or decrease undr HP...
11 December 2016 9,323 1 View
I want to do the modelling and simulation for additive manufacturing process. What are the simulation softwares for the Thermo-metallurgical-mechanical conditions in precise additive...
21 November 2016 6,051 18 View
few specimens are been taken with variation in size (by increasing primary dimension i.e. a x b x c, a+d x b x c, a+2d x b x c etc.), now the specimens are processed upto certain temp. (above...
22 September 2016 1,668 2 View
what changes occur in plots if one test a material (tensile test), if one applies the same strain rate in all?
22 September 2016 714 6 View
I want the stress strain behavior output by using the LAMMPS code. I have taken a specific size (100 x 50 x 100) size dimension of CuZr metallic glass with r (fcc) =3.61. the specimen was...
07 June 2016 3,891 3 View