I am trying to dope sulphur into Graphite Oxide and P123 using various amounts of Na2S.9H2O followed with hydrothermal washing and calcining.

When I run EDS on the samples, there seems to be no sulphur at all, what would be the problem? Or does anyone know how I could improve my experimental procedure, please?