i) Does the addition of hexachloroethane (degaser) brings any property change to the composite material cast?
ii) Similarly i would like to know the effect of addition of grain refiners in the melt?
Addition of Degaser should not lead to property changes.
Addition of grain refiner will introduce internetallic particles to the melt which acts as heterogeneous nucleating sites during solidification and result in decrease in grain size.
This causes degassing of Al-melt with a consequent minimization of porosity in the casting. In addition the grain refinement effect is also observed.
I intend to utilize a 2-inch plant, since it takes about a year for a plant to grow from the root. So, I must remove the native microorganisms (that is already present in the plants and their...
28 April 2024 3,055 2 View
Hi all, I have used the standard MKHS composition to make this buffer. The initial pH of the solution was 7.7. I adjusted the pH to 7.3 with 1N HCL and bubbled with carbogen (95% O2 and 5% CO2)...
13 September 2023 3,052 3 View
In a thick cylindrical pressure vessel, what are all the types of stresses acting on them? and tell that magnitude of various stresses acting on thick cylindrical pressure vessel in decreasing...
08 January 2021 7,550 0 View
Nuclei isolation from Pancreas? All the nuclei that I have isolated look good but they are all clumped together in some sort of gelatinous matrix? Does anybody have any inputs to improve the...
03 April 2020 8,187 2 View
extraction techniques
31 January 2020 7,426 1 View
Hello all, I am currently working on pellet induction in Trichoderma sps. for the production of cellulases. Although I am able to induce pellets of somewhat uniform size and compactness in a...
08 April 2019 9,589 0 View
Hello, Had anyone used antibodies from Signalway, Sabbiotech, USA for western blotting?. If so, kindly gives your comments about the quality of primary antibodies.
29 July 2018 2,191 1 View
Hi, For example, I have a 500*500 size of image, but I normalized the range of [0 1], then how to find the image actual coordinate value from the normalized image value
08 February 2018 2,525 4 View
i need some clarifications for dye extraction method. i am working in TiO2 dye sensitized solar cells.
09 January 2018 7,550 3 View
Dear Researcher (s) Can any one suggest the reference book for Data Analytics?
11 December 2017 6,308 2 View
I need to model an anisotropic material in which the Poisson's ratio ν_12 ≠ ν_21 and so on. Therefore, the elastic compliance matrix wouldn't be a symmetric one. In ANSYS APDL, for TB,ANEL...
09 August 2024 5,048 2 View
I am working on Abaqus/Explicit(Quasistatic ) for the deformation of the auxetic structure model. Please explain how the plastic input value should be considered from the true stress-strain curve...
05 August 2024 454 3 View
Sure, here is the translation: I have a 3D orthogonal woven composite structure where warp, weft, and binder yarns are oriented in three directions. After modeling these yarns and the matrix in...
28 July 2024 8,169 0 View
I am looking to purchase a photography kit for onsite metallurgical investigations, such as capturing photos of worn areas, hot tears, cold tears etc. Could anyone suggest me a good...
22 July 2024 3,490 2 View
I make polycrystalline diamond with tape casting followed by HPHT sintering. When i sintered the samples up till May, the sintering was good. When i sintered the samples in June and July at the...
16 July 2024 3,212 5 View
It is required to make a precursor gel for a SAPO-11 Zeolite, the compounds are the following: * As a source of Al: Aluminum Isopropoxide (98%) Formula: C9 H21 O3 Al PM: 204.24 g/mol Density:...
01 July 2024 617 3 View
I am doing orthogonal cutting of aluminum. My forces are changing according to mass scaling. How to decide the scaling factor?
01 July 2024 3,749 0 View
I am very new to the material modelling in GDIS. So, I want to learn how to model a nanostructure specifically core-shell in GDIS.
28 June 2024 5,224 0 View
I am doing 2D orthogonal cutting simulation in ABAQUS for aluminum. Reducing mesh size up to 0.08 mm reduces the error to 3% but further reduction leads to increase in error from 3 to 39%. Why I...
23 June 2024 9,080 0 View
I am preparing polycrystalline diamond (PCD) with tape casting. The powder is 8~12 um. After drying of tapes, I place several tapes in Ta cup without warm-pressing. Next, debinding is carried...
23 June 2024 7,758 2 View