It is required to make a precursor gel for a SAPO-11 Zeolite, the compounds are the following:
* As a source of Al:
Aluminum Isopropoxide (98%)
Formula: C9 H21 O3 Al
PM: 204.24 g/mol
Density: 1.035 g/mL
* As a source of P:
Orthophosphoric acid (85% by weight in H2O)
Formula: H3P O4
PM: 98 g/mol
Density: 1.685 g/mL
* As a source of Si:
LUDOX SM colloidal silica (30% by weight suspension in H2O)
Formula: O2 Si
PM: 60 g/mol
Density: 1.22 g/mL
* As Organic Agent:
Dipropylamine or DPA (99%)
Formula: C6 H15 N
PM: 101.19 g/mol
Density: 0.738 g/mL
*Deionized water
Formula: H2O
PM: 18 g/mol
density: 1g/mL
The desired molar ratio of the gel is as follows:
1 Al2O3 : 1 P2O5 : 0.4 SiO2 : 1 DPA : 40 H2O
What is the amount of g and/or mL of each component needed to prepare 60 mL of precursor gel?