I have synthesized convert graphite to graphene oxide(GO) and then GO to reduced graphene oxide(rGO) using the modified Hummer method. During PXRD characterization I found that GO XRD peak comes very intense, sharp but rGO XRD peak comes weak, less intense and broad. Why?