In plant scale trials we have obtained in excess of 82% yield using 60+ton batch crystallizers. We are changing the temperatures at various points of the cooling curve to push for higher yields.
We have tried various settings and seem to gave hit a plateau at 82% olein yield. Can anyone give suggestions on how we should approach the cooling in order to obtain higher yields