05 November 2019 0 8K Report

Hi there,

Could anyone please share the deposition conditions that they had used to thermal evaporate 80-100nm of gold? I'm struggling quite a bit with this. I've done several runs varying the current and deposition (25A and 45A) for (30mins to 2 hours) but have not observed any deposition. Unfortunately the thermal evaporator I'm using does not have a crystal thickness monitor so cannot real monitor the deposition thickness/rate in real time. Any comment would be much appreciated