I assembled the LFP and NCM full coin cells with SiO anode. After assembly their OCV was arround ~50uA, After resting for 12 hrs it shows negative OCV.
What could be the reasons?
Stirr the electrolyte and try with it or change i got the same when i did full cell
Asif Raza did you solve the problem?
Abir Hassan Talukder Not yet.. I think this is due to the electrolyte problem. I could not check it due to limited resources at the moment.
A crude extract of fungal culture using EtOH was subjected to column and TLC and partially purified compound was obtained. UV vis spectrum of the compound/s has max absorbance at 218nm. The...
11 August 2024 9,801 2 View
i am unable to interpret why its increases in start as shown in figure
11 August 2024 2,179 1 View
I am attempting to conjugate PEG to an amino acid at the C-terminus, for the purposes of producing nanoparticles. I have been told that PEG modified with amine groups can be used for this purpose,...
31 July 2024 2,033 1 View
We are working on a robot that cleans solar panels using fresh water supply and a rotating brush. We are trying to conserve as much water at possible by recycling the dirty water that is collected...
28 July 2024 5,778 2 View
Am trying to develop a lesson/lab to determine and compare antioxidant properties of soybeans of various colors. Preference would be low tech and low cost. Any assistance is greatly appreciated.
25 July 2024 7,498 2 View
In running two-dimensional gel electrophoresis on bacterial protein, some spots that appear to match a protein sequence have a significantly more acidic isoelectric point than the calculated pI....
24 July 2024 8,076 3 View
I intend to get an economical and accurate LAB TEST to measure arsenic concentration in blood sample.
23 July 2024 3,654 2 View
Their is new research published in the biological control journal, and I am one of the authors. I want to add it to my account at researchgare. How can I do this?
21 July 2024 7,545 0 View
I have read that it is better to use other research methods alongside document analysis for triangulation, although it can also be used as a stand-alone method.
18 July 2024 4,218 0 View
I am conducting a study on Effectiveness of e-content on academic achievement of secondary school science student.
17 July 2024 5,633 4 View
I tried four trials of the same Copper Phosphides sample in Alkaline medium ( 0.5M KOH) with Hg/HgO reference electrode and Pt as counter electrode. I used 0.001 V/s scan rate for first three...
10 August 2024 3,629 1 View
I am working in fungal fermentation of soybean meal and there is bacterial growth in them at times. I am trying to quantify fungal cell counts and bacterial cells; but I haven't been able to do at...
07 August 2024 7,535 4 View
Previously when I co-coluture anti-CD19(FMC63) CAR-Jurkat with Raji with E:T=5:1, Jurkat can eliminate Raji in 24h. However, when I test another CAR construct, although I can dectect totally CD69...
06 August 2024 641 2 View
i have sorted anti-NP specific plasma cells from bone marrow of C57BL/6 mice at certain times after immunization with variable counts and isolated total RNA using TRIZOL method for RT-PCR using...
05 August 2024 8,835 1 View
Hello, everyone. I have tried to determine carrier motilities of some materials, by Density Functional Theory, using Quantum ESPRESSO. There are a few methods to do it, like a package called...
04 August 2024 8,894 1 View
Hi, I am isolating monocytes from the bone marrow using the Mouse Monocyte EasySep kit. I want to treat these cells and monitor expression of specific markers over the course of 10 days. I will...
04 August 2024 7,282 2 View
I have been using paraffin, but the deposited ZnO still detach from electrode. What is the best binder to modify graphite paste electrode with ZnO nanoparticles?
03 August 2024 4,624 3 View
I have used PE and PE-Dazzle 594 fluorochromes and have managed to get NK cells to properly show GranzymeB expression after 4 hr PMA/ionomycin stimulaton, but for some reason my CD8 cells in the...
01 August 2024 7,677 2 View
What types of mask designs for metal deposition, to be used in a PVD system, are best suited for perovskite-based solar cells?
31 July 2024 4,835 3 View
Hi there! I recently started working on Lx-2 cells. When I thaw the cells, they start attaching within few hours but later in about 2 days they started rounding and dying. I used DMEM+2% FBS...
31 July 2024 3,893 0 View