Hi, I have exfoliated a mixture of graphite, pluronic f127, and water via Silverson shear mixer and after that I wanted to characterize the results via TGA. I want to show that after hours of exfoliation, Graphene exists in the precipitate and this can be illustrated in the TGA results where the weight percentage decrease clearly compared to the TGA results of graphite (the weight percentage barely decreases). My question is, after 4 hours of exfoliation, the weight percentage shows a small decrease from 100% to 97%. Any suggestions on what to do? I need the weight % of graphene (product of exfoliation) to clearly decrease in the TGA characterization.

Note that I used Nitrogen N2 in my TGA characterization. Should I use air flow instead of nitrogen flow? Thank you.