I can see some changes in property after kept samples in open environment for about a month.
Thank you in advance
Dear Artur sir, " Why do you want to store WO3 films ? "-- because I need to do I-V measurement later.
keeping samples in desicator with drying agent might prevent the H2O pick up process.
thank you for your response, Sir
Dear Thomas Sir, I can't do the measurement right after the deposition as for measurement and even for growth I depend on other lab. but keeping your suggestion in mind I will try to do it as quickly as I can.
thank you sir.
Hello everyone. I have conducted the research on post harvest longevity of tomato crop using plastic packaging and different doses of chemicals as two different factors. The design of experiment I...
28 February 2021 8,189 3 View
Related work experience plays a vital role in motivating the Entrepreneurship. But when we talk about high tech entrepreneurship in Aviation industry, we talk about very high investment and high...
22 February 2021 376 5 View
I have synthesized the peptide using Fmoc based solid phase peptide synthesis. Also I have cleaved the peptide from the resin and lyophilized it, but later realized that, I forgot to deprotect the...
21 February 2021 4,537 3 View
When doping in case of semiconductor is concerned, we doped Si by trivalent or pentavalent impurity atoms to improve its electronic properties but in case of nano-particles, sometimes we doped...
31 January 2021 7,128 1 View
As it is well known fact that nano-particles can easily aggregate during nucleation/ synthesis part due to high surface energy..by reading literature, I came to know that surfactants can help to...
30 January 2021 8,206 6 View
I am doing electrochemical oxidation of organic compounds for the the synthesis of nitrocompounds from simple organic molecules. I want remove supporting electrolyte after electrolysis. Please...
03 January 2021 7,858 2 View
Greetings everyone, I am learning to analyze multi-year and environment crop data using Meta R/ Adel R. But at some point during the process some errors were continuously observed and I could not...
18 December 2020 6,285 7 View
Nanodrop result of my DNA samples extracted from fresh finger millet leaves showed 260/280 ratio ranged from 1.7-2.2 whereas 260/230 ratio ranged from 1.1-2.2. How can I assess the quality of such...
30 November 2020 8,689 6 View
I got bright yellow coloured Schiff base after 6 hour reaction time. So i kept it for slow evaporation. Solvent was methanol. But after complete evaporation my product colour changes from yellow...
17 November 2020 3,824 2 View
Hello everyone, I am having trouble isolating and purifying an extracellular protein which I have expressed in E.coli. I have induced my protein at 0.5 mM IPTG by incubating it at 37 degrees for...
02 October 2020 8,223 3 View
When I conducted the degassing experiment using decompression under anaerobic condition(and I used ferrous based chelating agent), the oxidized ferric were observerd. So, could you tell me the...
03 March 2021 4,892 5 View
Favourable conditions of base pressure, rate of deposition. Also, by which characterisation technique to be used to verify the thickness of the deposited film.
28 February 2021 3,640 3 View
24 February 2021 2,362 5 View
As it is highly probable that pellets will have a higher degree of air gaps and voids than thin films, is it possible to pole the samples with corona poling nevertheless? Or is there the...
24 February 2021 1,349 1 View
I am trying to reduce graphene oxide by thermally but I have no proper information regarding this. Can any one help me regarding the details about temperature and time for the reduction of...
23 February 2021 4,155 4 View
I am trying to characterize an electrochromic system. The system uses ITO electrodes on glass, WO3 as the electrochromic film, and NiO as the ion storage layer. When I deposit NiO and WO3 and...
23 February 2021 9,592 2 View
I want to deposit multilayer coating of germanium and silicon monoxide on silicon wafer using ebeam evaporation?
21 February 2021 2,141 3 View
I want to measure the thickness of aluminum oxide and titanium oxide layers deposited on textured glass substates. The layer thicknesses are typically below 100nm.
21 February 2021 5,465 4 View
What does the color of a spiro-ometad film indicate? I got purple, green, red, even black color of the spiro film. Is there anything we can get from the preliminary color analysis(e.g. oxidation...
21 February 2021 1,831 4 View
I have done Uv-vis characterisation of my thin film and have received absorbance and transmittance data. Now I want to calculate the absorption coefficient but I dont know the thickness of my...
21 February 2021 7,148 8 View