That the capacitance retention rate reaches after 5000 cycles reaches 500% of its initial value by using GCD. Is this because the electrode material improves with the number of cycles?Does this result affect the publication of the research?
It is generally because of the least dipping time given during stability testing. Before starting the stability test, you should provide at least 4 to eight hours of dipping time. If the result is still that high, it will be due to the wettability factor as explained in our articles, "DOI: 10.1039/D3RA07788H and Article Novel MoS2-Sputtered NiCoMg MOFs for High-Performance Hybrid...