thickness of 0.1mm Mg target
Dear Hari U a . Yes. See the following useful links: https://www.deltamicroscopies.com/produit/magnesium-mg-sputter-coater-cathodes/
https://www.emsdiasum.com/microscopy/products/vacuum/targets.aspx
Good day! Maybe following links will be helpful:
https://www.labtech-em.com/em/magnesium-sputtering-target-dia-54-x-01mm-disc-9999-mg
https://www.abletarget.com/magnesium-sputtering-target/
https://www.quorumtech.com/wp-content/uploads/2020/08/Q150GB_Brochure.pdf
En suivant toutes les étapes mentionnées sur (ajouter une recherche) il me signale erreur, ressayer, j'ai essayé plusieurs fois, sans succès, toujours il me signal erreur, ressayer
02 August 2024 9,719 1 View
As one can read in numerous papers on this matter, the dislocation density is derived from the dependence of peak broadening on the diffraction angle, that is, on considered reflections. Thus, to...
28 July 2024 6,496 5 View
with secondary data collected from central bank to know the impact of digitalization in banks profitability, how can its impact be more precisely measured through econometric tools.
21 July 2024 7,295 10 View
I try to understand the ESP mechanism working. What kind of sensors it has, Is it necessary to modify or boost its mechanical ?
15 July 2024 4,772 1 View
Mangroves were reported to eat into limestone atolls like so much cake - but could it have been diatom partnerships at mangrove roots that ate into the rock? If gypsum formation is a clue, how...
12 July 2024 159 2 View
This question seeks to address the growing concern of cloned academic journals, which are fraudulent duplicates of legitimate publications. It aims to guide researchers, scholars, and academics on...
10 July 2024 5,966 2 View
Hi, Just curious to know that in chromatography, a chromatogram should be zoomed to what scale? 10 times of output , 50X or ..? Is there any regulation or general chapter which describes this?...
03 July 2024 3,119 6 View
I am working on one protein which gets aggregated (similar to alpha-synuclein and tau) in certain neurodegenerative diseases. I am trying to confirm the aggregation using Western blotting....
30 June 2024 5,060 3 View
Dear colleagues, I would be grateful to anyone who can answer my two questions: 1. Do the proportions of the shark's body change after drying? In other words, is it possible to discriminate two...
30 June 2024 6,101 3 View
Please, can any one inform us about risks of graphene and graphene oxide as a factor of cancer growth?
28 June 2024 6,815 4 View
I have been getting a low plasma and no coating while doing rf sputtering of copper doped ZnS using a power of 140 watts and at pressure of 6.5x10-3 Mb.
07 August 2024 4,526 4 View
I am experiencing this for the Bi2Se3 sputtering target. Initially, even if the target was 2:3 in Bi : Se, with a few sputtering runs, due to the high escaping tendency of selenium, the top layer...
23 July 2024 1,649 1 View
Hello I want to know about the sputtering condition of depositing FTO from target 95:5%. I tried with RF sputter in pressure 2.5Pa and 100 sccm Ar at room temperature but it showing no...
21 July 2024 1,680 2 View
We are fabricating a tandem structure where a ~50 nm thick WO3 film is deposited between two metal films using DC sputtering. We use a mixture of Ar and O2 gases at different flow rates while...
01 July 2024 2,686 2 View
I am fabricating the Hall bar (5 micron width and 35 micron length) of Ta(3nm)Co(4nm)Pt(5nm) using photolithoghaphy and sputtering. This Hall bar is connected by contact pads of Ti(10nm)/Au(60nm)...
29 June 2024 2,079 3 View
Using magnetron sputtering with an alloy target composed of A:B:C in a 2:1:1 ratio, the resulting thin film composition is A:B:C=1:1:1. How can you achieve a A:B:C=2:1:1 composition? What are some...
24 June 2024 1,605 0 View
We have observed many holes on the surface of TiO2. These holes have a diameter of approximately 1 µm and a depth of about 30 nm. The formation of these holes is mainly related to the...
20 June 2024 3,861 1 View
I conducted GIXRD measurements after performing O2 plasma treatment on a Cu surface. It was observed that the baseline is significantly high at low angles (10-30 degrees). What could this...
18 June 2024 2,996 3 View
Hello I am encountering Fe and other stainless steel (SS) element contamination in my LiCoO2 RF sputtering depositions. I suspect the source is the "etching" of the magnetron stainless steel frame...
11 June 2024 2,196 3 View
I have prepared Copper thin films by magnetron sputtering and the samples have been annealed at 100, 200 and 300 degree celsius. The variation of the rms roughness and all other AFM height related...
11 June 2024 9,774 1 View