I obtained silk from bombyx moori after lithium bromide treatment. The aqueous solution I get solidifies when I try to mix the drug in it using magnetic stirrer which is very difficult to use for electrospinning. How can I get rid of the problem?
In addition to the previous suggestions, you have to check the effect of pH of the drug solution and whether it contains certain salts which may affect the physical properties of the final solution.
Arun Karthick I dewaxed the silk cocoons in aqueous sodium carbonate solution at a temp of 100 for 30 min. After drying the silk at 37 C, I am trying to dissolve it in THF but no result after 12 hrs stirring.