What is the role of current vs. time in galvanostatic deposition of Platinum? Is it possible to accelerate the deposition rate from a very dilute plating solution, by increasing the applied...
04 April 2016 6,742 6 View
If a thin gold layer (50 nm) is sputter coated on a wafer, is it possible to make this Au layer negatively charged, for example by adsorbing a negatively charged specie? Can we citrate for this...
01 January 2015 8,202 3 View
In the case of sputter coating, if we switch from Platinum (density 21.45 g/cm3) to Copper (density 8.96 g/cm3) for the same thickness of 20 nm, how the metal density difference will affect the...
10 October 2014 2,568 5 View
I have noticed poor adhesion between sputtered Au and Pt thin films. Why this is so, and is there a way to enhance this adhesion?
10 October 2014 9,409 14 View
Can I use colloidal graphite coating as working electrode for the electropolymerization of conductive polymers? e.g. PANI, PEDOT, PPy.
09 September 2014 6,016 4 View
I am trying to do potentiostatic electropolymerization of aniline but the reaction does not take place at all. Can an old Ag/AgCl reference electrode be the reason which was not in use for many...
09 September 2014 4,238 15 View
I wish to know the method and materials required to remove sputtered Ag or Au layer from the surface of a polycarbonate membrane used for the preparation of nanowires.
08 August 2014 1,844 5 View
While trying to deposit Ag, as soon as I dip an Ag/AgCl reference electrode into a Ag deposition solution of 0.2M AgNO3 + H3BO3 + HNO3, white colored matter starts to produce from the interface of...
08 August 2014 784 27 View
In order to check proper working of my potentiostat, I have performed CV of 10 mM potassium ferricynaide/ferrocyanide redox couple in 0.5M KNO3 (figure attached). An Ag/AgCl reference electrode...
07 July 2014 1,676 26 View
I want to determine if a particular metal can be electrochemically deposited on another in the form of thin film.
07 July 2014 7,378 12 View
I would like to have an opinion about microscopy techniques to distinguish between folded and unfolded protein molecules belonging to a same or different proteins.
06 June 2014 9,117 3 View
I want to sequentially deposit uniform layers of Cu, Ni, Fe and Zn, respectively on a gold layer. Is such sequential deposition possible galvanostatically?
06 June 2014 6,634 5 View
Cyclic voltammetry of potassium ferricyanide in a microfluidic chip containing integrated gold working electrodes and ITO as the counter electrode leaves brown spots at the working electrode...