Hello,

I am spin coating a non-polar monomer onto a PDMS layer, with the coating solution made up of chloroform. The concentration is very low. However, I keep getting a hole in the middle of the film using dynamic dispense. Is there any way to remedy that without doing additional surface treatment onto the PDMS layer?