26 September 2014 2 8K Report

Has anyone spin-coated polyethylene (medium density) onto SiO2 surface? What is the conditions to get smooth homogeneous film? For example concentration of PE, solvent, spin speed.

I follow the procedure in this paper:

http://www.nature.com/nature/journal/v434/n7030/abs/nature03376.html

"medium-density polyethylene in decalin was spun at 190 °C onto the substrates and annealed at 90 °C for 3 h. Root-mean-square roughness of the dielectric interface produced in this way is 24 Å (2 times 2 microm)"