Are there any method in order to improve the crystallization properties of indium tin oxide (ITO)?
William .. appreciate it .. it is an interesting idea to approach ..
Amit .. I did ITO by sputtering .. thin films ITO less than 200nm thickness ..
Deposition pressure and substrate temperature are the most important parameters.
Besides transfer length method (TLM) and CTLM, is there any practical method that can be used to measure the specific contact resistance (Ohm-cm2) of metal-semiconductor contact?
11 December 2015 1,047 4 View
01 January 1970 1,237 5 View
Favourable conditions of base pressure, rate of deposition. Also, by which characterisation technique to be used to verify the thickness of the deposited film.
28 February 2021 3,640 3 View
24 February 2021 2,362 5 View
As it is highly probable that pellets will have a higher degree of air gaps and voids than thin films, is it possible to pole the samples with corona poling nevertheless? Or is there the...
24 February 2021 1,349 1 View
I am trying to characterize an electrochromic system. The system uses ITO electrodes on glass, WO3 as the electrochromic film, and NiO as the ion storage layer. When I deposit NiO and WO3 and...
23 February 2021 9,592 2 View
I notice that upon washing and air-drying of my RGO/SPCE surface and characterizing again via DPV, the current response towards ferricyanide probe significantly decreases. My worry is that the...
22 February 2021 5,324 3 View
I want to deposit multilayer coating of germanium and silicon monoxide on silicon wafer using ebeam evaporation?
21 February 2021 2,141 3 View
I want to measure the thickness of aluminum oxide and titanium oxide layers deposited on textured glass substates. The layer thicknesses are typically below 100nm.
21 February 2021 5,465 4 View
In the PVD of TiN thin films (~100A), I've found the resistivity of the TiN films dropped from ~100 to 60um*cm with N2 flow increasing up to the metallic mode ending point; then the resistivity...
21 February 2021 1,864 2 View
I have used Picral etchant (4.2 g Picric acid, 10 mL Acetic acid, 70 mL Ethanol, 10 mL distilled water) but it didn't work. Is there any alternative?
21 February 2021 2,558 5 View
I have done Uv-vis characterisation of my thin film and have received absorbance and transmittance data. Now I want to calculate the absorption coefficient but I dont know the thickness of my...
21 February 2021 7,148 8 View