Can anyone suggest me a simple method to determine silicon to aluminium ratio in zeolites.
Determination of Si/Al molar ratios in microporous zeolites using calibration-free laser induced breakdown spectroscopy.
You can use X-ray fluorescence analysis or another way to dissolve zeolite for chemical analysis in a mixture of HCl and HF.
By using EDS analysis.
Hi, I am using GROMACS 5.1.4 to simulate water in contact with a surface. I am only interested to calculate some properties of water near the surface. Let's say at a distance of x nm from the...
03 March 2021 9,989 2 View
Which solution reveals the microstructure and features of nickel-based alloys?
02 March 2021 2,221 3 View
Which tools can be used to generate machine codes for additive manufacturing?
02 March 2021 7,220 2 View
For my experiments, I have to express ectodomains of human CD28 and CD3z. As a source, I extracted RNA from Jurkat cells and verified the quality of RNA on the gel. I, then, prepared cDNA using...
23 February 2021 7,051 4 View
The continuity boundary condition is automatically created for a shared (common) surface boundary but I want to have it for an edge. Please help me out. In image 8 is the base of the cylinder and...
05 February 2021 3,459 2 View
anyone can help me to explain what is direction Vector 1 and direction Vector 2 in porous media when modelling in ANASYS fluent
01 February 2021 6,866 1 View
When we are doing sampling by means of simple systematic random sampling,how do we calculate the design effect for use during calculation of sample size for our work?
20 January 2021 5,328 3 View
I am developing a solver to simulate compression of oil in shock absorber filled with viscoelastic compressible oil. The model will consider the loss due to viscosity which will decide the...
15 January 2021 1,707 1 View
sphericity test in Repeated Measures ANOVA
05 January 2021 6,177 4 View
can anyone suggest that the above is a genuine journal for technical publication...
04 January 2021 4,388 9 View
Incompletely cross-linked pdms are difficult to remove.
01 March 2021 798 3 View
We have deposited silicon carbide on carbon substrate using one PVD technique. Due to amorphous behavior of SiC at low deposition temperature, we performed heat treatment of those films at...
22 February 2021 2,072 3 View
21 February 2021 3,417 5 View
Hi everybody, please, can someone tell us if the transition metals (W, Fe, Ni, etc ...) in silicon destined for solar cell manufacturing can be detected by ED-XRF technique. Note that the...
18 February 2021 6,231 4 View
Hello, I am observing a nearly periodic background spectrum for a wide variety of SERS substrates. I see this response (attached below) for bare Au films, Cu films, and Au nanoparticles on...
15 February 2021 9,922 5 View
My design contains three parts. A silicon rubber membrane is placed between upper and lower part. I want to calculate sound transmission loss by using comsol Multiphysic. There are lots of...
05 February 2021 466 4 View
First of all, whether it is possible to identify the presence of water and its amount on the Silicon substrate by using only FT-IR spectroscopy. Can ATR-FTIR spectroscopy find out the wettability...
03 February 2021 9,085 4 View
I have been trying to make an even PEDOT: PSS (PH1000) film with the doctor blade technique (tape casting) with varying results. I have been using a silicon substrate that's treated with piranha...
01 February 2021 8,506 5 View
I would like to generate multiple large samples of amorphous silica in LAMMPS. Currently I am generating it by beginning with a lattice of silicon and oxygen atoms and using a melting and...
28 January 2021 6,128 4 View
Hi Everyone, I made some polymer(Polylactide) films on Silicon wafer. The polymer was dissolved in DCM and THF. I observed that the colour of the film at the centre of the Wafer is different...
27 January 2021 9,724 1 View