I made KNN nanofibers, using recipe is TCD 5cm, Voltage 11kV, flow rate 0.75ml/h, around 22.6 degrees, and 16%hum.

But, the rainy season is coming, RH became 28 degrees and 45%hum.

When I tried to make electrospun same KNN solution with the same electrospinning condition, nanofibers were solidified early and hanged on the collector as seen in picture..

I tried changing Voltage to 7~11kV and TCD to 3~5cm, but the results were same..

How can i solve this problem..? I can't wait untill the rainy season is over.. and I can't change solution's concentration..

More Hyunjung Cho's questions See All
Similar questions and discussions