I am making PVDF/ TiO2 solution for electrospinning. I have DMF and Acetone as solvents, so can you tell me the optical conditions for this process (ratio, temperature, time and stirring speed) ?
Nguyen Nga, I suggest first mixing TiO2 with solvents and homogenizing it for 10-15 minutes. After this, add PVDF to the solution at room temperature and to make it clear solution stirring needs around 8 h.