i have prepared PMMA polymer using PMMA beads mw 350000
using chloroform as solvent at 40 degree C. and poured in to glass petri- dish. And kept 24 hrs. for drying in room temperature. After drying, the film is not free standing and its not delaminating from the glass petri-dish. Plese help me to prepare PMMA polymer sheet.