2 Questions 5 Answers 0 Followers
Questions related from Shruthi K N
i have prepared PMMA polymer using PMMA beads mw 350000 using chloroform as solvent at 40 degree C. and poured in to glass petri- dish. And kept 24 hrs. for drying in room temperature. After...
02 September 2021 8,483 2 View
solution casting method.