I'm using corn grits with added 5% moisture, hydration for 1h before extrusion process.
The final parameters
Screw speed : 160
Feed rate: 50 r/m
Temperature profile: 40-80-120-165-175-175
Water pump rate: none
Max Pressure: 165pa
What modification needed to increase the pressure, and thus getting a more desirable extruded product ?