I have alumina and AlN powder mixture (maximum particle size should be 300nm) and I have 3mm Agate balls, after ball milling process what would be the final particle size that I can get.? does it have any ratio or formulla?
probably you will have no "real" milling but only de-agglomeration as your agate milling balls are actually much softer than the material you want o mill and have a low density and therefore low impact. Moreover you will produce a lot of silica debris which may contaminate your sample.