I am using HMBA-MBHA (1% DVB) resins for the solid-phase synthesis of peptides, which will be the best way to swell these types of beads? (I would like to know the time duration and solvents that can be used)
Dear Poornima Dineshika Herath Mudiyanselage ! The best swelling agent for 4-(Hydroxymethyl)benzoyl-4-methylbenzhydrylamide resin copolymers is acetone. But you need to understand what is the purpose of the project? https://www.peptide.com/resources/peptide-synthesis-resins/cleavage-from-hmba-mbha-resin/