11 November 2016 2 746 Report

etchant for insitu metallography  or Replica metallography for austenitic steel.it found to be very difficult to find good and fast etchant to use in replica. I tried 1:1 HCl:HNO3, water based aqua regia(2:1:1=HCl:HNO3:H2O). also please describe procedure for prepration?