21 December 2016 3 5K Report

I want to prepare Graphene Nanoplatelets (GNP) solution in ethanol for a coating process. I want to achieve a well-dispersed GNP solution and I have GNP with me. I also want to make it in the least time possible. The best possible combination I found on surveying research papers was 0.05g GNP in 20 mL ethanol sonicated for 2 hours. However that is not very practical given the amount of GNP solution I require. Does anybody know of any other conc/time combination which can be achieved by ultrasonication. 

One advantage is I do not require dispersion for long amount of time: maximum stability for 3 days.