C=0.23%,
Mn=0.66%
Ni=2.9%
Cr=1.29%
Mo=0.24%
01 February 2016 7,547 3 View
pure iron powder by electrolysis
31 December 2015 972 1 View
Self Repair of Active Metals
02 March 2015 5,960 0 View
C=0.23%, Mn=0.66% Ni=2.9% Cr=1.29% Mo=0.24%?
11 December 2014 1,686 0 View
polymer wear
10 November 2014 4,126 0 View
06 July 2014 1,055 3 View
If the density of a polymer composite increases, what is the effect on the electrical conductivity of the material?
01 February 2013 5,485 3 View
Practical application of percolation threshold.
08 September 2012 1,008 16 View
Material should be like glass
07 August 2012 2,694 2 View
What is the effect of modulus of elasticity of Ni & Cr on steel hardness and how is its hardness different as modulus of elasticity changes?
07 August 2012 7,793 1 View
I looking for ferro calcium production process
03 March 2021 1,755 4 View
Hello everyone. Given microstructure image belongs to a 12% ledeburitic cold work tool steel (annealed and tempered). The sample was etched with picral (100 mL ethanol and 4 g picric acid). I...
02 March 2021 4,119 3 View
It is oftentimes said to be a distinctive metallographic trait that differentiates a fully austenitic and a fully felly ferritic steel without etching that might distinguish between two. Why...
02 March 2021 728 2 View
As I was tweaking step-by-step OpenCalphad6 Macros step1.ocm involving phase and thermal property calculation of a High-speed steel, I could not incorporate more than 6 elements in the steel...
01 March 2021 8,840 1 View
I have a structure that employs d-ring swiveling tie-downs that corrode during use and become "frozen". I have sample swivel assemblies that I wish to corrode to see if I can free them using one...
01 March 2021 3,739 3 View
I am conducting anodic electrodeposition of MnO2 onto a stainless steel substrate, using a platinum strip as a counter electrode. This is done galvanostatically, with the current held between 5...
27 February 2021 1,829 3 View
My main concern is that the metal powders should not weld to the mold surface and I should easily be able to eject out the pressed samples. I am looking for alternative for graphite moulds. The...
22 February 2021 2,965 4 View
Dear all, If steel jacketing is used to retrofit a reinforced-concrete (RC) column, can we use it to improve flexural strength? I understand that we leave gaps between the ends of the jacket and...
22 February 2021 1,906 5 View
Hi all, Does SeismoStruct support modeling rectangular RC columns retrofitted with steel jackets (e.g. rectangular, elliptical) ? Any suggestions for other software (apart from...
20 February 2021 4,521 1 View
I tried to sweep my ferroelectric devices from -2V to 2V and then from 2V to -2V and The two hysteresis peaks are off by several microFarads. Should i increase bias voltage? I am doing these...