we want to conduct the flexural test of aluminium alloy composite.Could anybody provide the specimen dimensions based on ASTM standard.
Hello Saty Dev
A varying specimen shapes and sizes can be used for this test, but the most commonly used specimen size is ASTM D790 is 3.2mm x 12.7mm x 125mm
(Thickness x Width x Length)
Good luck
PVR
Dear PVR Thanks for your contribution.
Actually our concern is to know the standard for Aluminium Alloy not for plastics. If you have any idea for the same please share it.
Use ASTM D7264
Use ASTM E290-14 and E190-14
Actually, I am working with Al-B4C- Al2O3 hybrid composites. I have performed the operation by utilizing the wire EDM process to my developed composites. I found alloy 6061 as a base matrix having...
21 January 2021 7,381 3 View
I want to prepare bacterial media containing Kraft lignin ( dissolved in 0.1 M NaOH). after I autoclave,the lignin gets precipitated. Please suggest how to retain the solubility of lignin in the...
07 December 2020 800 3 View
I am doing social constructionist research on everyday life. There are so many books on qualitative research that it is hard to decide which one is among the top best ones. I am searching for a...
12 May 2020 328 3 View
In fermentation when the broth is gradually becomes viscous what will be the most relevant method for biomass measurement. as it becomes difficult to separate the actual biomass from the other...
22 December 2019 7,864 3 View
Hi everyone I have been working on U-Pb geochronology of accessory phases mostly zircon, monazite, rutile, titanite and apatite. I would like to know how I can do common Pb correction using...
11 December 2019 8,806 1 View
Though, the fused deposition modeling (FDM) technology is very old and widely used to fabricate plastic parts. it does not give the significant surface quality of products. The anisotropy is also...
15 September 2019 5,982 3 View
I have prepared carbon dots (CD) using plant material and got its absorbance maxima at 231 nm through UV-Vis spectrophotometer. Then what should be excitation maxima of Carbon dots during its...
28 November 2018 4,796 6 View
I have a deep groove ball bearing (NSK make). I wish to introduce artificial faults in the outer race and inner race such that I can study their signal characteristics. I am facing two...
26 November 2018 2,974 3 View
Actually i have prepared carbon dots using lactose and checked its fluorescence by preparing carbon dots solution in distilled water. then, another carbon dots solution was prepared in distilled...
25 October 2018 1,799 3 View
Actually I want to find the particle size of B4C powder, Al2O3 and Mg powder by particle size analyzer using a solvent. But I am facing problem to select the appropriate solvent for the same. I...
30 July 2018 1,342 1 View
We use reactive sputtering process to make aluminum nitride film, and want to make c-axis aluminum nitride film on a silicon substrate, but the crystal orientation cannot be seen with...
03 March 2021 7,975 3 View
Which solution reveals the microstructure and features of nickel-based alloys?
02 March 2021 2,221 3 View
For wrought alloys soaking time at solutionizing temperature is determined by thickness .Do we have such standards for cast Al alloys
23 February 2021 8,839 3 View
I have prepared Ag-Cu alloy with polymer coating upon it.... how can I measure thermal conductivity of it ?
22 February 2021 5,915 3 View
I need to carry out molecular dynamics simulation on Aluminium alloy. For this i need the crystal structure that which could be further replicated to form a structure.
22 February 2021 1,410 1 View
I have used Picral etchant (4.2 g Picric acid, 10 mL Acetic acid, 70 mL Ethanol, 10 mL distilled water) but it didn't work. Is there any alternative?
21 February 2021 2,558 5 View
I have given Elastic and Superelastic material properties, but I think we need to provide the damage parameters also. Please help me here.
16 February 2021 8,694 1 View
Are there alternatives to the Devarda alloy when estimating nitrogen? devarda alloy is reducing the nitrate to ammonium
15 February 2021 8,838 3 View
14 February 2021 2,157 3 View
How can we quantify metastable phases like martensite in Ferrous and Titanium alloys, in relation to their stable counterpart For example in EBSD, XRD, Optical? Eg, Martensite and Ferrite maps.
09 February 2021 7,572 3 View