We are coating 24k Gold on ceramics with TiN, the gold color is not beautiful with deep color, Gas ratio is 200sccm(Ar)/500sccm(N2)-(3min)/(5min).Is this ratio necessary. to tweak???Thank!!
So it looks like problem, possibly vacuum chamber inside is dirty (there is thick layer of condensate on walls). Second is reduced performance of vacuum system (it may be necessary to add oil to steam-oil pump) to check the system for pumping speed and obtaining ultimate vacuum.