I have successfully coated the Fe304@Sio2@PPy( Polypyrrole) simply by taking 100mg Fe304@Sio2 ,suspended in 15 ml DI water then sonicate for 15 min then add 100 microlitre pyrrole. Solution was cooled to 0 degree celcius. Then APS solution in water was added dropwise and polymerization continued for 10 hr. I did the characterization of the compound and it seems to be successful.

In the similar way i want to coat the lonic liquid on Fe304@Sio2. It also has pyrrole on it so i want to coat and polymerize it on Fe304@Sio2. I repeated the same procedure but i was unable to coat. The problem is i have pure but only 0.19 g of IL. Does any one have idea how i can do it?