I prepared films based on CMC (Carboxymethylcellulose) and anionic clay (Hydrotalcite MgAlNO3). The problem is that I can not remove the thin film from the glass petri dish.
Hello Arhzaf,
You can use polypropylene petri dish.
in heterogeneous catalysis we always need to determine the porosity (pore size and volume and specific surface area) of the solid materials synthesized in the laboratory, in order to find an...
08 September 2019 3,572 4 View
We use reactive sputtering process to make aluminum nitride film, and want to make c-axis aluminum nitride film on a silicon substrate, but the crystal orientation cannot be seen with...
03 March 2021 7,975 3 View
I try to check the uv-vis absorption of Indium nanoparticle. Now I am measuring in solution, can I measure it in the form of a film?
01 March 2021 930 3 View
Favourable conditions of base pressure, rate of deposition. Also, by which characterisation technique to be used to verify the thickness of the deposited film.
28 February 2021 3,640 3 View
24 February 2021 2,362 5 View
Hello everyone, I'm looking for a way to delaminate copper current collector of water-based anodes in Li-ion batteries without damaging the graphite film. I tried different materials such as HNO3...
24 February 2021 3,785 3 View
As it is highly probable that pellets will have a higher degree of air gaps and voids than thin films, is it possible to pole the samples with corona poling nevertheless? Or is there the...
24 February 2021 1,349 1 View
I am trying to characterize an electrochromic system. The system uses ITO electrodes on glass, WO3 as the electrochromic film, and NiO as the ion storage layer. When I deposit NiO and WO3 and...
23 February 2021 9,592 2 View
I notice that upon washing and air-drying of my RGO/SPCE surface and characterizing again via DPV, the current response towards ferricyanide probe significantly decreases. My worry is that the...
22 February 2021 5,324 3 View
I want to deposit multilayer coating of germanium and silicon monoxide on silicon wafer using ebeam evaporation?
21 February 2021 2,141 3 View
I want to measure the thickness of aluminum oxide and titanium oxide layers deposited on textured glass substates. The layer thicknesses are typically below 100nm.
21 February 2021 5,465 4 View