Hello everyone,
I want depositing thin films of ZnS using chemical bath deposition is there anyone could help me
Best regards.
sol-gel methode it's great to produce a thick films
Hi,
You can use our recipe. It was published on 2014 at the Materials Research Bulletin. We have deposited ZnS thin films grown by CBD free of toxic precursors. You can find our work in my ResearchGate profile.
Kind regards
Dear Carlos thank's
Best regards
khaoula best regards ;)
hello Khaoula
It is my pleasure to help you
my master was about deposition of ZnS nanostructure using CBD
what do you need to know?
you can cited our attachment article
Best regard
Raghad
How can the deposition time affect the carrier density concentration (electrodeposited thin film)
07 December 2020 7,954 3 View
I'm working on a systematic mapping in computer science subject. In the step of "Identification of Research", I choose to work with these digital libraries : IEEE Xplore, Scopus, Web of Science,...
12 February 2019 5,732 4 View
I need to know how to dilute the furan resin and how can i clean it. what solvent to use ( water and ethanol does not work well) .
12 December 2018 9,340 3 View
I can't find a solvent to extract my product from DMSO? I used a lot of solvent, the problem is that the solvent is miscible with DMSO or my product is not soluble in this solvent.
04 January 2015 3,612 18 View
What this unit identifies for the ion exchange capacity ca. 0.92 meq. g-1. I am a newcomer in the membrane area. I just started. I highly appreciate your help
08 May 2021 0 0 View
Anyone can recommend any books on such topics? Thanks in advance.
02 March 2021 8,457 2 View
(This statement is from wikipedia, BTW). What is so special about metallic bond that is limiting high-P low-T state of a matter (as long as individual atoms exist, not white dwarf of neutron star...
02 March 2021 3,309 2 View
The Lanthanide contraction which is the decrease in ionic radii of the elements in the lanthanide series from atomic number 57, lanthanum, to 71, lutetium, is due to poor shielding of the 4f...
01 March 2021 2,272 4 View
Hi all, I need to cleave the ester in Ethyl 2-amino-1H-imidazole-5-carboxylate to make the carboxylic acid and retrieve the product from solution to use in downstream applications of linking to...
01 March 2021 8,766 3 View
Favourable conditions of base pressure, rate of deposition. Also, by which characterisation technique to be used to verify the thickness of the deposited film.
28 February 2021 3,640 3 View
24 February 2021 2,362 5 View
As it is highly probable that pellets will have a higher degree of air gaps and voids than thin films, is it possible to pole the samples with corona poling nevertheless? Or is there the...
24 February 2021 1,349 1 View
Hi, I know the attached Txy diagram has an error but can't figure it out. Could you please look at the diagrams and explain it to me?
23 February 2021 4,239 1 View