Then I am thinking to use that Pt deposited carbon paper as a counter electrode for CO2RR in flow cell setup.
You may stick PTFE tape on one side of carbon paper and peel it off once the electrodeposition is done.
H2PtCl6 should be ok.
Dear Anil Kumar you can use square-wave potential (SWP) method for electrodeposition of Pt using chloroplatinic acid hexahydrate. It is the most often used method for controlled and reproducible Pt morphologies.
Which solution reveals the microstructure and features of nickel-based alloys?
02 March 2021 2,221 3 View
Which tools can be used to generate machine codes for additive manufacturing?
02 March 2021 7,220 2 View
I am searching for a good place for the Post Doc,
02 March 2021 4,053 3 View
Working on chandrayaan-2 DFSAR data, there are three datasets available: 1) Slant range image data product: The slant range complex image file. Each pixel is represented by two 4-byte floating...
02 March 2021 8,481 3 View
Hello, The Cranet website does not provide any lead to the data obtained from their multinational survey on HRM practices. Any help on accessing the data would be most appreciated. Thank...
01 March 2021 9,536 3 View
I am looking for anti-nuclear antibody (ANA) and anti-Phospholipid antibody ELISA kit for Non Human Primate serum samples. Any suggestions highly appreciated. Thank you.
28 February 2021 6,512 3 View
Is there any book chapter/book, webpage or research article available to understand genome-wide gene identification?
28 February 2021 8,095 1 View
For an overfit data set the cross validation error will be much bigger than the training error. Is it true or false?
23 February 2021 3,616 2 View
In my opinion, the RG site is useful in solving scientific problems and shows the researcher's ability. Besides, the separation of the H-index from the self-citations and the overall index is an...
22 February 2021 3,894 6 View
I performed a Proton NMR of graphene powder prepared by electrochemical exfoliation technique. It shows some peaks. But I can't understand it.
21 February 2021 8,947 3 View
I am using a Sutter electrode holder for my patch clamp experiments, but I'm having trouble keeping positive pressure inside my electrode due to a leak out of the back of the holder. I have added...
02 March 2021 5,829 1 View
I want to do RF sputtering of ITO on glass substrate using magnetron sputtering. what thickness do i need to make it good conductive layer to use it for PSC. Moreover, whats about thickness of...
01 March 2021 395 3 View
Dear All, I want to quantify carbon deposition on the surface of the CuZnAl catalyst. I have tried thermogravimetric analysis, but I've got weight gain as the active Cu- get oxidised. Does anyone...
01 March 2021 1,907 3 View
I am a student of MS Environmental Engineering and started my research phase. I am working on metal removal ( chromium iii ) by using activated carbon prepared from the agricultural feedstock. So...
01 March 2021 5,475 2 View
I am conducting anodic electrodeposition of MnO2 onto a stainless steel substrate, using a platinum strip as a counter electrode. This is done galvanostatically, with the current held between 5...
27 February 2021 1,829 3 View
Dear all, I am trying to perform a MD simulation about the interaction between CO2 and a polymer. I create my model, solvate it and perform the NVT and NPT equilibration. Now I am not able to...
26 February 2021 10,014 3 View
During performing CV of a GCE or modified GCE, we rise the potential in the first half of the cycle and reduce it in reverse half. During the first half, what is the nature of charge on GCE or...
25 February 2021 7,994 3 View
Has anyone ever tried to deliver CO2 with a CGA 300 regulator? I know that a CGA 320 regulator is standard for CO2. The issue is that I currently do not have any free CGA 320 regulators. I also...
25 February 2021 3,292 3 View
Respected Professor's i hope you are doing well and happy. i need some information about carbon Nanotubes. before blending the CNT with the matrix the CNT has been introducing in some treatments....
24 February 2021 5,383 5 View
I am trying to characterize an electrochromic system. The system uses ITO electrodes on glass, WO3 as the electrochromic film, and NiO as the ion storage layer. When I deposit NiO and WO3 and...
23 February 2021 9,592 2 View