I want to solder a Aluminium 1000 series tube to a Tin coated CRCA Steel Plate. At present the flux I'm using is not properly wetting the Aluminium tube surface and there are small holes present in the joint leading to leakages.
Two choices. 1 a bit of Zn (5%) in 50/50 HCl as flux and tin solder or 2 for higher yield straight Zn as solder. HCl/Zn as flux is gassy so fume hood
/M
I want to obtain continuous High Voltage DC from regular 9V Battery or household AC supply connection. How to convert LV DC or AC to HV DC?
11 December 2017 5,184 7 View
04 May 2017 2,963 4 View
I conducted tensile and flexural tests for 4 different anisotropic materials (Fibre reinforced plastic). I got tensile strength of material C higher than material N. Whereas, higher flexural...
10 November 2016 2,435 7 View
08 September 2015 3,100 1 View
I looking for ferro calcium production process
03 March 2021 1,755 4 View
Hello everyone. Given microstructure image belongs to a 12% ledeburitic cold work tool steel (annealed and tempered). The sample was etched with picral (100 mL ethanol and 4 g picric acid). I...
02 March 2021 4,119 3 View
It is oftentimes said to be a distinctive metallographic trait that differentiates a fully austenitic and a fully felly ferritic steel without etching that might distinguish between two. Why...
02 March 2021 728 2 View
Is the electropolymerisation of polyaniline coating over stainless steel (SS) via Cyclic voltammetry technique is really adherant? Else how to improve the adhesion of the coating, whether any...
01 March 2021 8,220 2 View
As I was tweaking step-by-step OpenCalphad6 Macros step1.ocm involving phase and thermal property calculation of a High-speed steel, I could not incorporate more than 6 elements in the steel...
01 March 2021 8,840 1 View
I have created an Ice 1h crystalline structure and an Aluminium substrate structure and equilibrated both at 250K. Now I need to bring them together in a way that an adhesive bond is created....
01 March 2021 3,325 2 View
I have a structure that employs d-ring swiveling tie-downs that corrode during use and become "frozen". I have sample swivel assemblies that I wish to corrode to see if I can free them using one...
01 March 2021 3,739 3 View
I am aiming to determine the ADC values of a commercial fish feed, but I do not have a steam pelleter or extruder available to me. Ideally, the pellets could be coated with some inert marker....
28 February 2021 7,967 3 View
Do we immerse the bricks horizontally or vertically ? #bricks#waterproofingsurface#civil#engeenering#chemicalengineering#wax#parafinwax
28 February 2021 6,685 2 View
I want to use 0.1% gelatin. Should that be made in PBS or sterile water? Should I autoclave the gelatin soln after making it in water/PBS?
28 February 2021 274 2 View