when I deposit copper sulfide on FTO glass, it separate easily
my dear,this link maybe help you
http://pubs.rsc.org/-/content/articlelanding/2015/ta/c5ta00068h#!divAbstract
thank you
I cant increase my temperature and the time for annealing TiO2 paste . what should be temperature and time until my paste answer?
03 April 2017 6,659 0 View
my question is about kind of semiconductor
10 November 2016 7,059 6 View
I want to do RF sputtering of ITO on glass substrate using magnetron sputtering. what thickness do i need to make it good conductive layer to use it for PSC. Moreover, whats about thickness of...
01 March 2021 395 3 View
Any idea on how to get the volumic ratio of glass fiber in a gypsum board ? Thank you for your help !
01 March 2021 2,501 3 View
I am looking for datasets similar to this one: http://archive.ics.uci.edu/ml/datasets/Concrete+Compressive+Strength I am looking for concretes with different types of aggregates (Recycled,...
27 February 2021 6,801 3 View
I'm building a cfx model of thermoplastic pultrusion process on ansys and i have a doubt on how is the proper way to set this parameter in a porous medium
24 February 2021 1,915 1 View
Hello everyone, I'm looking for a way to delaminate copper current collector of water-based anodes in Li-ion batteries without damaging the graphite film. I tried different materials such as HNO3...
24 February 2021 3,785 3 View
I'm doing a cfx simulation of a multiphase flow in pultrusion and i set the Interfacial Area density in the heat exchange of a porous medium in this way IAD=Total fiber lateral surface of fiber...
23 February 2021 6,043 1 View
I want to measure the thickness of aluminum oxide and titanium oxide layers deposited on textured glass substates. The layer thicknesses are typically below 100nm.
21 February 2021 5,465 4 View
I am working on polishing abrasives. I need to do few characterizations ? which can provide the on time surface chemistry of substrate with polishing abrasive during optical polishing. I would...
18 February 2021 5,319 3 View
The regenerated cellulose film was prepared by zinc chloride/H2O system. The zinc chloride had been washed away in the regeneration process, and the wet film which was not dried had uniform...
18 February 2021 9,538 1 View
Regarding my needs I am looking for a glass coating agent that makes the glass hydrophobic permanently
09 February 2021 3,924 5 View