Hi all,
I want to import the residual stress profiles along the rolling and transverse direction into the Deform and also extrude those over the whole plate. Would you be able to point out how to do that?
Regards,
Panos
I am looking for thick-sectioned plates (of the order of 2000m x 500mm x 120.00mm thick)
01 February 2018 2,105 3 View
I have a 30 mm thick plate AA7050 alloy and I want to reduce the residual stresses without altering the microstructure; so I cannot heat up the specimen. What techniques are out there? Is it...
01 February 2018 7,779 1 View
I am inspecting some machined specimens and I noticed not all grains and misorientations can be seen in the 3 IPF maps; while Euler mapping reveals quite well both -even though there might be some...
31 December 2017 2,755 4 View
In most cases, scientists design a low yield deformable matrix which strengthens via phase transformations, twinning etc. However in many engineering applications a low yield point is not desirable.
31 December 2016 6,447 3 View
I am using a 2707 waters HPLC device. When I try to inject a sample, it says missing plate or rack. I changed the needle and calibrated its position but I still get the same problem. I even get...
02 March 2021 1,408 1 View
We have HUVEC bought from Invitrogen. Cat no -C-003-5c. while first plating the cells we have bought the protocol suggests not to centrifuge the cell with media to remove the DMSO. Should we...
02 March 2021 3,713 2 View
Good afternoon, I recently used OmniLog from BIOLOG for my experimentations : I tested the metabolism of different strains on 2 types of plates. I have 16 strains of 3 different groups...
02 March 2021 3,584 1 View
I want to do a parameter study of a aixsymmetric cylinder in Abaqus. I want to create several jobs where I get the stresses for 3 different points in my model. These points are defined. I wrote a...
01 March 2021 10,078 1 View
Hi. I am doing non linear FE analysis using a new material beam under flexural 2 point loading using ANSYS. I have defined a bilinear material model. The solution has converged. In results I am...
01 March 2021 9,911 3 View
We have always used the 96 welled plate, the 48 welled plate but apparently there is much evidence on the 24 welled plate and above all its benefits.It states it is the same you would use on ELISA...
28 February 2021 1,149 1 View
Hi, recently I encountered a protocol for plating which was not the usual method I have been practicing (pour LB agar onto plate, allow it to solidify, pipette bacterial suspension onto plate,...
28 February 2021 7,292 3 View
for all the rheology researchers, my question is, how relevant is a mini slump cone (smaller than a standard 50 cent rheometer). currently based on testing, the thickness of slumped material is...
26 February 2021 3,668 1 View
Hello, recently I am having some difficulties with maintaining the cell culture of primary cells isolated from a skin biopsy (normal and malignant). The coating of culture plates with Matrigel (a...
26 February 2021 6,151 2 View
25 February 2021 6,760 1 View