Dear researchers,

I want to add alpha-tocopherol to chitosan film forming solution to prepare chitosan film with alpha-tocopherol. First I added tween 80 as an emulsifier to chitosan film-forming solution(2%) at concentrations of 50, 75 and 100 percent of alpha-tocopherol that then was added to chitosan film forming solution at different concentrations of 0.1, 0.125, 0.15 and 0.2 percent of the solution. Then, it was homogenized with ultra turax at 13000 and 27000 rpm and dried in petri dishes at oven( 30 D. of celsius). Unfortunately, all prepared films showed greasy surface and non-uniform structure. Can any researcher help me how can I prepare a better film with uniform structure? 

Similar questions and discussions