I'm not looking for spesific alloys. The answer I am looking for is more general:
For example:
"3xx, 4xx for LPDC; 2xx, 5xx for HPDC"
I'd like to ask you to share me the source as well.
Hi. I hope the following article could help you:
http://www.aimnet.it/allpdf/pdf_pubbli/6_05/Bonollo.pdf
Dear Artunc
The AlSiMg alloy ,i.e,. EN AB 43000 ,would be used for LPDC.In contrast, AlSi alloy,i.e, 47100 would be used fot HPDC.
May be helpful to you:
https://www.european-aluminium.eu/media/1526/aam-manufacturing-1-casting-methods.pdf
Hello dear colleagues, We have prepared a manuscript on NiTi-based alloys and are seeking a second opinion on our current TEM results. If you are a Ph.D. holder with experience in TEM and have...
07 August 2024 9,563 0 View
How select composition for ods-high entropy alloys?
31 July 2024 2,795 1 View
Any suggestions with respect to etchant composition and holding time?
27 July 2024 6,925 2 View
The catalytic effect of retained austenite refers to the phenomenon wherein quenching steels with a small amount of retained austenite, when subjected to tempering at a specific temperature...
27 July 2024 8,508 0 View
I am working on powder metallurgy, and during the compaction process, the powder does not pelletize and remains in its powder form. To address this issue, I am considering using binders to improve...
13 July 2024 9,003 2 View
Waspaloy is considered the benchmark alloy. Due to the different gamma prime solvus temperatures, we couldn't adopt the same double aging treatment. Can anyone suggest how to select temperatures...
13 July 2024 2,417 1 View
In the expression for solid solution strengthening model that has been widely used in the literature use a linear form consisting of strength coefficient, and concentration of elements in wt.%....
11 July 2024 4,476 3 View
It is required to make a precursor gel for a SAPO-11 Zeolite, the compounds are the following: * As a source of Al: Aluminum Isopropoxide (98%) Formula: C9 H21 O3 Al PM: 204.24 g/mol Density:...
01 July 2024 617 3 View
I am doing orthogonal cutting of aluminum. My forces are changing according to mass scaling. How to decide the scaling factor?
01 July 2024 3,749 0 View
Using magnetron sputtering with an alloy target composed of A:B:C in a 2:1:1 ratio, the resulting thin film composition is A:B:C=1:1:1. How can you achieve a A:B:C=2:1:1 composition? What are some...