I would like to perform in-situ XRD studies using Anton Paar's HTK 1200N heat temperature over chamber in 10%H2+90%Ar gas mixture until 1000 deg C. Whether it is safe to work under these conditions?
Thank you Fernando, I have inquired Anton Paar about this issue. They have suggested me not to use any reactive gases with these system because their furnace housing is just made of alumina. However, inert gases can be used without any problem