except BSA and in printed screen electrodes
Can you please elaborate more?
Based on my current understanding, you intend to block the nano-gold surfaces; if so, then you can go for any other proteins.
Proteins strongly bond on the gold surface due to surface energy, intermolecular forces, hydrophobicity, and ionic or electrostatic interaction
High density polymers can also be used.
Nachiket Gokhale ok, proteins and polymers are good. but witch one is better and why? I want to know which one blocks better?
Dear Professors, Colleagues and Friends I need to develop a simple Matlab/Simulink model of reverse droop controller for a simple LV MG. How can I get a simple one to use it as a sample? A basic...
22 February 2021 8,647 2 View
I am working on a biosensing project on paper substrate, however, it is found that the RNase contamination occurs on the filter paper. Might I ask is there any method to clean the paper surface...
12 February 2021 3,926 3 View
I want to run 5 different models to estimate stream flow. In order to optimize the characteristics of these models I use Taguchi method. So I have to run different models according to the Taguchi...
11 February 2021 7,986 6 View
Hi everyone, I would really appreciate it if someone can tell me when and why a raw fluorescence starts below zero. In the picture attached below the blue colour curve starts from a negative...
09 February 2021 4,642 3 View
This is a follow-up on an earlier question regarding mechanistics of vaccines: why current vaccines don't block transmission. In summary, they don't engage mucosal immune cells to produce IgA....
08 February 2021 8,321 3 View
In Abaqus I know that there are two methods for incrementation (Automatic and fixed incrementation). I want to control the incrementation by myself. I want to input the values of load increment...
03 February 2021 6,943 3 View
Dear all. I'm modeling the RC column with cyclic displacement by Abaqus-Explicit. The concrete model used Concrete Plastic Damage model. However I'm facing with a error about the excessive...
01 February 2021 7,726 1 View
I am facing a problem that cellular debris observed in my SHSY5Y cells. I have seeded the cells in DMEM media with 10% FBS in T-25/ 60mm dish (antibiotic used PEN-Strepand gentamycin). I have also...
17 January 2021 3,074 3 View
I modeled a simple crack in abaqus. I get J-integral as output as well as components of stress intensity factor KI, KII, KIII. However, I do not know how to get GI, GII and GIII. I searched in...
04 January 2021 1,783 2 View
Conventionally, the process of Stage II fatigue crack growth is governed by Paris law with less microstructural effect. When fatigue crack growth test was carried out for pearlitic steels ( both...
03 January 2021 7,075 3 View
I notice that upon washing and air-drying of my RGO/SPCE surface and characterizing again via DPV, the current response towards ferricyanide probe significantly decreases. My worry is that the...
22 February 2021 5,324 3 View
I am working with a material which is sensible to water and oxygen, I would like to oxidize this powder either chemical or electromagnetically. Does anyone knows a method to electrochemically...
09 February 2021 2,944 3 View
Hi, I am working on a multi cationic material that has Li in it. I wish to measure the conductivity of my sample. We have a 3 electrode system with Ag/AgCl as a ref, platinum, and glassy carbon...
29 January 2021 405 2 View
I am trying to measure resistance from I-V curve from a chemiresistor/ FET sensor with a keithly sourcemeter. The substrate is soaked/ wet with protein and phosphate buffer only. But the I-V line...
24 January 2021 8,009 3 View
For electrochemical sensors, the electroactive surface area (ESA) show higher value for the working material as compared to bare (reported in several papers). My bare electrode is FTO and working...
17 January 2021 7,220 3 View
My Hg/HgO electrode was used for EIS test in 4M NaOH solution. I found something in the salt bridge. After that, my EIS results found the noise at a low frequency (tested in a faraday cage)....
16 January 2021 1,900 1 View
I am trying to quantify Parylene C's hermetic encapsulation quality using EIS with a 2 electrode configuration (WE/WS and RE/CE). I am simply using two patterned gold layers on glass as my...
12 January 2021 7,399 14 View
In In potentiostatic EIS, we do measure the current at the WE. Do we apply the ac + dc signal on the reference electrode or the counter electrode ? for impedance calculation , do we calculate...
10 January 2021 6,275 2 View
Anodizing of SS304 creates a thick oxide layer on that. Is this layer non-electrical conductive? What thickness should be obtained in order to make the surface non-electrical conductive?
01 January 2021 3,359 4 View
Hope so, you are all fine, I want to perform EIS and CV of my material Carbon doped Titania as a counter electrode for DSSC, I just want to know what electrolyte solution and in what molar...
25 December 2020 7,095 3 View