What is the optimum ratio of steel fibre used for production of geopolymer concrete?
It depends on the goal of what property you want to improve. Use of about 2% by volume will improve the ductility of the geopolymer concrete
hello everyone; I have a review paper I want to check it for plagiarism before I submitted to the journal, any one could help me I will be grateful.
09 October 2018 5,801 2 View
I have a review paper in geopolymer concrete, i need suggestions for good journal with fast publication.
02 March 2018 5,045 6 View
I am trying to simulate vehicular loading on an orthotopic steel deck bridge section in ABAQUS software. The red arrow mark in the attached figure indicates the direction in which the vehicle will...
08 August 2024 719 0 View
I have modelled a steel structure using beam elements in Abaqus and attached to this structure reinforced concrete slab. The analysis that I am making is heat transfer of the structure. The...
07 August 2024 1,028 0 View
Machine learning (ML) has shown great potential in predicting the compressive strength of concrete, an important property for structural engineering. However, its practical application comes with...
03 August 2024 2,546 2 View
Suggest one of them 1. Teflon-lined stainless steel autoclave: 2. Alumina (Al2O3) ceramic container
30 July 2024 7,326 1 View
The catalytic effect of retained austenite refers to the phenomenon wherein quenching steels with a small amount of retained austenite, when subjected to tempering at a specific temperature...
27 July 2024 8,508 0 View
How can the rubber fibres produced by the electrospinning device be removed from the fibre collector (aluminium foil) without affecting the orientation of the rubber fibres for use in reinforcing...
26 July 2024 8,281 0 View
Please investigate the effect of temperature and strain rate of hot deformation and the formation of delta ferrite in martensitic stainless steel 410?
25 July 2024 9,408 0 View
I have tried to saturate ferritic steel with hydrogen using the electrolytic method and H2SO4. However, the effect was very poor even after 3 days of "saturation". Can anybody help in choosing a...
24 July 2024 4,393 2 View
I am working on scale development in behavioral finance by undertaking a mixed-method approach using the exploratory sequential design. The phenomenon has diverse meanings in existing literature...
20 July 2024 9,153 11 View
I am simulating interlocking / dry stacked masonry in Abaqus. I am using a friction coefficient of 0.6 for my model as it is stated in the previous research as well as in the base paper. The...
16 July 2024 5,047 0 View