I want to make dehydrated PU solution for coating nano-silicon, which reacted with water. Is it possible to get alcohol based PU solution? Any paper or suggestion will be appreciated....
Hello dear, you can use the prepolymer method. If you send your mail, I might send you an information.
Thanks Prof Murillo. My email address is : [email protected]
What is the reason for changing color of the paraffin based PCM upon prolonged heating at around 142 Deg C.
09 October 2019 8,756 5 View
We have prepared silicon powder, which contains 30 nano to 9 micron range. We checked around 35% of particles are less than 1 micron. We want to separate these 35% particles from the rest. Any of...
08 September 2018 7,653 4 View
I like to know, how can we give super-hydrophobic finishing during HTHP dyeing of polyester fabric. I've heard that such finish give a permanent super-hydrophobic finish on polyester fabric. If...
07 August 2018 4,007 1 View
Hi I'm searching good electrically conductive polymer. Do you know any such polymer available in the market?
31 December 2016 5,317 3 View
Hi I like to know, is it possible to deposit silicon on cotton fabrics using vapor deposition method? I shall be glad, if you kindly share any related paper.
06 July 2016 8,701 3 View
I'm interested to know, whether there is any formula to determine the maximum strength of a yarn for different counts, different materials and staple length...
10 November 2015 985 7 View
Is it possible to develop copper-silver alloy? Is there any work on this? I want to know alloy only for copper and silver, no other metals..If any of you has done research on this, pl. let me know...
03 April 2015 7,361 3 View
We are searching for some fire-retardant chemicals, which gives permanent fire retardant property, but will NOT affect the natural hydrophilic property and permeability of cotton fabric. Could...
31 December 2014 8,762 4 View
How can I determine a good adhesion strength range for coatings on polymer surfaces, such as DLC on polymer substrates? Is there a specific threshold for adhesion strength (from T-peel tests)...
10 August 2024 942 3 View
I did PR spin coating on trench structure. I used AZ P4620 PR and the thickness or PR is around 11um. The substrate is Si. And my trench structure depth is 141um(negative way). Even though I...
08 August 2024 2,298 0 View
I have been getting a low plasma and no coating while doing rf sputtering of copper doped ZnS using a power of 140 watts and at pressure of 6.5x10-3 Mb.
07 August 2024 4,526 4 View
I am trying to coat my micelles and PLGA based nanoparticles with cell membrane using an Avanti mini extruder according to literature . I use 200nm membrane but my particles end up to be 400nm And...
30 July 2024 3,294 3 View
Your comments
28 July 2024 2,822 2 View
I am trying to coating metal oxide into steel substrate, for better sticking planning to utilse epoxy based, Could you please suggest suitable curing agent for the coating purpose
25 July 2024 438 3 View
Novel areas especially
24 July 2024 8,416 0 View
I have been harvesting monocyte-derived macrophages from buffalo and cattle fresh whole blood using the same protocol for years and getting good macrophage cultures. Below is the protocol that I...
23 July 2024 4,074 2 View
I have immunized BalB/C mice with a protein using the intradermal (ID) method with Complete Freund's Adjuvant (CFA) and Incomplete Freund's Adjuvant (IFA), following a 14-day interval and three...
22 July 2024 9,160 2 View
Dear Participants- Faculty and Researchers from Pakistani Higher Education Institutions, Thank you for participating in research study that aims to 'Analyze Individual and Institutional Factors...
18 July 2024 7,024 1 View