Recently, the erosion rates have been doubled and excessive glowing chunks of carbon fabric are seen in the stream of plasma flow. Is it matrix (phenolic resin) dominated property? Is it due to trapped moisture during curing of carbon/phenolic composite? What precautions/ testing must be conducted to ensure better and smoother ablation during testing?