What is the dielectric strength of highest practical vacuum in the range 10^-9 torr to 10^-12 torr, if the electrodes are smooth Pt (W=5.4 eV) ?
Hi Thomasz,
20...50 kV/mm and depends on the absolute pressure and electrode form. Maybe that helps: https://web.archive.org/web/20120301112907/http://www.htee.tu-bs.de/forschung/veroeffentlichungen/giere2002.pdf
regards
Erik
It would have to have transparent leads and deep sub-lambda geometries of photosensitive elements.
01 January 1970 2,263 1 View
If I put charge q onto an electrode, it will not be more than neutralized by the charge due to polarization of a ferroelectric. My email: [email protected]
01 January 1970 2,504 2 View
I am using a Sutter electrode holder for my patch clamp experiments, but I'm having trouble keeping positive pressure inside my electrode due to a leak out of the back of the holder. I have added...
02 March 2021 5,829 1 View
I want to do RF sputtering of ITO on glass substrate using magnetron sputtering. what thickness do i need to make it good conductive layer to use it for PSC. Moreover, whats about thickness of...
01 March 2021 395 3 View
I am working on roof joint and trying to simulate the behaviour in Abaqus. I am successful in running the model but the final graph does not follow the experimental curve in the negative direction...
01 March 2021 6,661 3 View
I am currently doing my third year design project. I have been assigned to design a glycerol recovery column in vinyl acetate monomer production. The process unit before the recovery column is an...
01 March 2021 9,525 4 View
I am looking for datasets similar to this one: http://archive.ics.uci.edu/ml/datasets/Concrete+Compressive+Strength I am looking for concretes with different types of aggregates (Recycled,...
27 February 2021 6,801 3 View
I am conducting anodic electrodeposition of MnO2 onto a stainless steel substrate, using a platinum strip as a counter electrode. This is done galvanostatically, with the current held between 5...
27 February 2021 1,829 3 View
During performing CV of a GCE or modified GCE, we rise the potential in the first half of the cycle and reduce it in reverse half. During the first half, what is the nature of charge on GCE or...
25 February 2021 7,994 3 View
I am trying to characterize an electrochromic system. The system uses ITO electrodes on glass, WO3 as the electrochromic film, and NiO as the ion storage layer. When I deposit NiO and WO3 and...
23 February 2021 9,592 2 View
Dear all, If steel jacketing is used to retrofit a reinforced-concrete (RC) column, can we use it to improve flexural strength? I understand that we leave gaps between the ends of the jacket and...
22 February 2021 1,906 5 View
What are the testing rate for electrodes recommended by ASTM for cochlear implants. I am currently doing the 15mm/min elongatio testing.
22 February 2021 1,515 1 View