Does anybody have the piezoelectric measurement systems for thin films?
What is the thickness of your samples...
Thank u for your reply...... it is a polymer thin film... i can coat it in different substrates... thickness will be 300 nm to 1 microns...
You have to do PFM for this. We have piezo measurement unit but it work for bulk samples only.
thank you.... what is the minimum thickness for measuring piezo response in your facility?
The basic thing is, we can measure stand alone film. But we don't have facility for measuring piezo constant with substrate. So, 100 micron would be measurable in our sample holder.
Thank you.....
A crude extract of fungal culture using EtOH was subjected to column and TLC and partially purified compound was obtained. UV vis spectrum of the compound/s has max absorbance at 218nm. The...
11 August 2024 9,801 2 View
How can I measure the thickness of thin film by Uv-Vis?
06 August 2024 7,810 3 View
Why is TLC not a form of partition chromatography and paper chromatography not a form of absorption chromatography?
03 August 2024 7,035 3 View
I need something like Camag's VisionCat software for photodocumentation of TLCs. Could you recommend something?
31 July 2024 8,415 1 View
Hello, I'm trying to measure the conductivity of semiconductor films but since I don't have a commercial four point probe set up I would like to build one on my own in my lab. I have generators,...
30 July 2024 906 2 View
My final research is about making chitosan/pva hydrogel for wound healing using gelatin as crosslinker. Last month, i made the thin film hydrogel and it turn well. It was okay. Last week, i make...
28 July 2024 2,794 6 View
I know that films and other low-thickness laminated products are produced using biaxial orientation, but is there something similar for sheets with a thickness of around 6 mm? Or are they...
21 July 2024 1,559 1 View
I work with planar interdigitated electrodes (IDEs). The finger width and the spacing between the fingers are 5 micron. The surface of the IDEs is coated by a non-conductive polymer layer...
16 July 2024 5,031 1 View
We're studying the stability and fusion behavior of multiple PVC compounds in a Brabender. After a few trials, we set the temperature at 195 °C and the rotor speed at 70 rpm. Samples differ in...
12 July 2024 2,768 1 View
I am facing a difficulty to prepare the thin film which contains fluorine contained silica monomer, as we know F is highly reactive with low surface energy and it could be the reason of low...
09 July 2024 6,017 3 View