I want to know how much of the silane is present on my PDMS surface after treatment.
FTIR is a good start and widely available. AFM can also be used, or XPS if it's available.
Thank you Dr.Reiserer.
For surface composition, XPS is better technique as you can get exact quantitative data.
Thank you all.
Hey all, I'm working on synthesizing Gold nanoparticles (GNP) - antibodies conjugates for biomedical purposes. We are struggling to find an efficient method to sperate the unconjugated antibodies...
03 March 2022 8,959 4 View
Hello! i´m trying to use the biodot zx1010 to make the test and control line on a lateral flow strip but the manual that came to our machine it isn´t the right one, and doesn´t have much...
25 January 2021 6,790 1 View
I have images with different channels, I would like to make a mountage of the single channels+the image resulting from the merging of them. in the attached images you can see the different...
06 August 2019 1,814 3 View
Hot plate temperature falling down/doesn't rise beyond a point. I'm running a TMAH etch of silicon in a 2000mL beaker with wafer in a teflon holder. The hotplate is set at 92C with the external...
03 October 2017 8,730 0 View
While cutting simulation the process is getting aborted due to excessive distortion of the mesh . What ALE frequency and remeshing sweeps must I consider to avoid this . I am using J-C model and...
01 November 2016 7,417 7 View
I have a PDMS microfluidic device with one channel (10mm X 5mmX 50 um) having an inlet (2mm diameter hole) and outlet (2mm diameter hole). I am trying to pass solutions through inlet and pulling...
21 April 2016 9,251 4 View
Also how to clean the silicon master after the pdms has been removed? PDMS residue is left behind.
20 April 2015 7,067 12 View
How can I determine a good adhesion strength range for coatings on polymer surfaces, such as DLC on polymer substrates? Is there a specific threshold for adhesion strength (from T-peel tests)...
10 August 2024 942 3 View
I did PR spin coating on trench structure. I used AZ P4620 PR and the thickness or PR is around 11um. The substrate is Si. And my trench structure depth is 141um(negative way). Even though I...
08 August 2024 2,298 0 View
I have been getting a low plasma and no coating while doing rf sputtering of copper doped ZnS using a power of 140 watts and at pressure of 6.5x10-3 Mb.
07 August 2024 4,526 4 View
Hi! So i attempted to understand a novel protein behavior towards heat application by analyzing its secondary structure change. I subjected the protein to a thermal denaturation analysis using...
06 August 2024 1,989 3 View
I am trying to coat my micelles and PLGA based nanoparticles with cell membrane using an Avanti mini extruder according to literature . I use 200nm membrane but my particles end up to be 400nm And...
30 July 2024 3,294 3 View
I went for Plackett Burman Design for selecting the optimization factors of growth conditions for pesticide degradation. I started with 7 parameters. But, after the experiments and analysis, only...
29 July 2024 5,015 1 View
In hirshfeld surface calculation i did not find any red spot in hirshfeld surface, is it ok for research article to write?
28 July 2024 2,988 0 View
Dear researchers, Why specific capacitance is not proportional to the specific surface area? I have material A with a surface area higher than material B, but material B is showing little bit...
26 July 2024 9,156 2 View
I am trying to coating metal oxide into steel substrate, for better sticking planning to utilse epoxy based, Could you please suggest suitable curing agent for the coating purpose
25 July 2024 438 3 View
I have been harvesting monocyte-derived macrophages from buffalo and cattle fresh whole blood using the same protocol for years and getting good macrophage cultures. Below is the protocol that I...