4 Questions 7 Answers 0 Followers
Questions related from Sasank Peri
Hot plate temperature falling down/doesn't rise beyond a point. I'm running a TMAH etch of silicon in a 2000mL beaker with wafer in a teflon holder. The hotplate is set at 92C with the external...
04 October 2017 8,716 0 View
I want to know how much of the silane is present on my PDMS surface after treatment.
17 November 2016 2,840 4 View
I have a PDMS microfluidic device with one channel (10mm X 5mmX 50 um) having an inlet (2mm diameter hole) and outlet (2mm diameter hole). I am trying to pass solutions through inlet and pulling...
22 April 2016 9,239 4 View
Also how to clean the silicon master after the pdms has been removed? PDMS residue is left behind.
21 April 2015 7,058 12 View