Up to what temperature can we carry out impedance analysis for an half cell (Electrode/GDC/Electrode) with GDC as an electrolyte in SOFC's?
Thank you for the response and the document Mr.Habib.
For a cell with symmetrical (identical) electrodes in an oxidizing atmosphere up to 900 C, in a reducing atmosphere about 600-700 C. For SOFC, also a maximum of about 600-700 C
Thank you very much Osinkin Sir.
At which sintered temperature can get a full cubic 8YSZ?
Literature says that at 950-1050 for 2-4 hrs the cathode ink adheres to substrate and results in desired porous micro structure. My samples adhere at 1200-1250oC resulting in dense micro...
02 March 2019 595 1 View
In the process of Electrode ink preparation we generally use binder solvent and glycerol at some wt ratios which are mixed thoroughly and coated on substrate to achieve required thickness. The...
08 September 2018 5,850 3 View
How does the applied pressure affect the ceramic pellets to be crack free. My pellets when pressed are crack free, but after sintering I find the pellets crack. what would be the reason?
09 October 2017 8,854 7 View
https://www.youtube.com/watch?v=bV41avoVXJU https://www.youtube.com/watch?v=v3l5Hm97TjY These videos give information in using the Match software for XRD and refinement calculations. I would like...
02 March 2015 1,643 0 View
Hi all, I am validating a polyclonal antibody raised against human ANT4, through WB and ICC. In most of my controls, the antibody shows very little off-target binding, but when I pre-incubate the...
03 March 2021 5,999 3 View
I need to prepare a solution of Napabucasin (inhibitor of cancer cell stemness) in dichloromethane. The drug is expensive, so maybe somebody already tried to do it. If it is soluble, what is the...
02 March 2021 9,945 3 View
I am using a Sutter electrode holder for my patch clamp experiments, but I'm having trouble keeping positive pressure inside my electrode due to a leak out of the back of the holder. I have added...
02 March 2021 5,829 1 View
im working now on TPV solar cells and metamaterials and i realy need our help in CST microwave i have a tpv cell simulation and i want to extract particullarly the absorbtion of only the active...
02 March 2021 2,246 2 View
I want to do RF sputtering of ITO on glass substrate using magnetron sputtering. what thickness do i need to make it good conductive layer to use it for PSC. Moreover, whats about thickness of...
01 March 2021 395 3 View
I am a little confuse with the mechanism of solid lipid nanoparticles (SLNs). The main point of encapsulating drugs into SLNs is because some drugs have low solubility in water. Therefore, SLNs...
01 March 2021 3,703 3 View
Favourable conditions of base pressure, rate of deposition. Also, by which characterisation technique to be used to verify the thickness of the deposited film.
28 February 2021 3,640 3 View
28 February 2021 2,534 2 View
I am conducting anodic electrodeposition of MnO2 onto a stainless steel substrate, using a platinum strip as a counter electrode. This is done galvanostatically, with the current held between 5...
27 February 2021 1,829 3 View
I diluted siRNA and RNAiMAX in opti-MEM and added to the cells which they were in the growth medium. Is it a right way? or should I culture cells in the opti-MEM medium for a while and not in...
26 February 2021 10,041 3 View